Color Changes in Dry Pigmented Tech-Sil25 Maxillofacial Elastomer after Artificial Weathering

Bunyan Shahad Fadhel1, Abood Akhlas Zeid2

1B. Sc Dent. Tech., Northern Technical University, Institute of Technology, Kirkuk, Iraq

2Assistant Professor, B. Sc, MSc, Dent. Tech., Middle Technical University, College of Health and Medical Technologies, Baghdad, Iraq

Online published on 27 November, 2019.

Abstract

Background

Maxillofacial prosthesis that processed from silicone elastomer materials have their own physical properties that will lead to degradation on frequent subjection to ultra violet sunlight that will need to replacement of the prosthesis because of its pigments undergo color changes.

Aim of the Study

The objective of this study isto evaluate effect of three periods of artificial aging at (75h, 150h, 300h) on color changes of room temperature volcanized (Tech-sil25) silicone maxillofacial material after incorporation 0.2% by weight of dry pigment (Burnt sienna) by using spectrophotometer test.

Materials and Method

Total of20 circular disk (2mm thick and 20mm diameter) specimens were fabricated by incorporation of 0.2% by weight of Burnt sienna to room temperature vulcanized (Tech-Sil25) silicon divided into two groups control and study group, 10 samples for each group. The control group samples wastested for color change with spectrophotometer and the study group were subjected to artificial weathering ultraviolet for (75, 150, and 300 h) then after each period they tested for color change with spectrophotometer. All data were analyzed with a descriptive statistical analysis, one-way ANOVA test, LSD test.

Result

Subjection of the burnt sienna pigmented (Tech-sil25) maxillofacial silicone elastomers to ultraviolet light resulted in a highly significant increase (P≤ 0.01) in mean values of color absorbance after artificial weathering for (150–300 hours) where there is no significant differences in mean values of color absorbance after artificial weathering for (75 hours).

Conclusion

The color change in silicone elastomer pigmented with burnt sienna is increase with increasing the aging period.

Top

Keywords

Color changes, dry pigmented, Tech-Sil25 maxillofacial, artificial weathering.

Top

 
║ Site map ║ Privacy Policy ║ Copyright ║ Terms & Conditions ║ Page Rank Tool
886,539,824 visitor(s) since 30th May, 2005.
All rights reserved. Site designed and maintained by DIVA ENTERPRISES PVT. LTD..
Note: Please use Internet Explorer (6.0 or above). Some functionalities may not work in other browsers.